AWS-klassifikaasje: AWS 5.9
BESKRIUWING:
RVS-lasstried hat hege bekledingseffisjinsje, goede lastechnyske prestaasjes by lassen yn alle posysjes. Se wurde in soad brûkt yn 'e yndustry: boustruktueren, auto's, brêgebou, mynboumasines, spoarwegen, oaljepipen, gasdrukdragende apparatuer, stroomfoarsjennings, ensfh.
MODEL NR. & GRUTTE:
1. Fabryksfoarsjenning OEM-tsjinst.
2. Model: ER308 ER308L ER308LSi ER309 ER309L ER316 ER316L ER316LSi ensfh.
3. MIG-triedgrutte: 0.8mm 0.9mm 1.0mm 1.2mm 1.6mm.
4. TIG-triedgrutte: 1.6mm 2.0mm 2.4mm 3.2mm 4.0mm.
YNLIEDING:
Wy leverje ferskate soarten roestfrij stiel lasdraad, ynklusyf Mig solide lasdraad, Tig-staaflasdraad en ûnderdompele-bôgelasdraad, allegear fan hege kwaliteit en wurde wrâldwiid ferkocht.
Utsein 308 en 309 biede wy ek 304, 321, 347, 316L, 310, 2209 en 201 oan. Lykas spesjale spesifikaasjes lykas 318L, 904L, 2594, NiCrMo-3, Ni1.
FERPAKKING:
Mig-lassdraadpakking (spoel- en trommelpakket)
Diameter: 0.8 - 2.0mm
Pakket: 1 kg/spoel, 5 kg/spoel, 15 kg/spoel, 20 kg/spoel, 100 kg/trommel, 200 kg/trommel
Tig-staaf lassen triedpakking (plestik buis)
Diameter: 1.0 - 5.0mm
Pakket: 5 kg/pak
Underdompele bôge lassen tried
Diameter: 2.5 - 5.0mm
Pakket: 20 kg/pak, 25 kg/pak
Neutrale ferpakking en OEM binne wolkom!
Gemyske gearstallingen fan roestfrij stielen lasdraad:
| Modelnr. | C | Si | Mn | P | S | Cr | Ni | Mo | Cu |
| 304 | 0.08 | 0.30-1.00 | 2.00 | 0.045 | 0.030 | 18.00-20.00 | 8.00-11.00 | 0.18 | 0.003 |
| 304L | 0.03 | 0.30-1.00 | 2.00 | 0.045 | 0.030 | 18.00-20.00 | 8.00-12.00 | ||
| ER307 | 0.04-0.14 | 0.30-0.65 | 4.30-4.75 | 0.030 | 0.030 | 19.50-22.00 | 8.00-10.70 | 0.5-1.5 | 0.75 |
| ER308 | 0.08 | 0.30-0.65 | 4.30-4.75 | 0.030 | 0.030 | 19.50-22.00 | 9.00-11.00 | 0.75 | 0.75 |
| ER308L | 0.03 | 0.30-0.65 | 1.50-2.30 | 0.03 | 0.02 | 19.5-21.5 | 9.00-11.00 | 0.75 | 0.75 |
| ER308LSi | 0.03 | 0.65-1.00 | 1.60-2.40 | 0.03 | 0.02 | 19.5-21.5 | 9.0-11.0 | 0.75 | 0.75 |
| ER309 | 0.12 | 0.30-0.65 | 1.00-2.50 | 0.03 | 0.03 | 24.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER309L | 0.03 | 0.3-0.65 | 1.5-2.3 | 0.03 | 0.02 | 23.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER309LSi | 0.03 | 0.65-1.0 | 1.6-2.4 | 0.03 | 0.02 | 23.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER316 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 18.00-12.00 | 11.0-14.0 | 2.0-3.0 | 0.75 |
| ER316L | 0.03 | 0.3-0.65 | 1.5-2.3 | 0.03 | 0.02 | 18.0-20.0 | 11.0-13.0 | 2.05-2.55 | 0.75 |
| ER316LSi | 0.03 | 0.65-1.0 | 1.6-2.4 | 0.03 | 0.02 | 18.0-20.0 | 11.0-13.0 | 2.05-2.55 | 0.75 |
| ER310 | 0.08-0.15 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 25.0-28.0 | 20.0-22.5 | 0.75 | 0.75 |
| ER347 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 19.0-21.5 | 9.0-11.0 | 0.75 | 0.75 |
| ER317 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.01 | 18.5-20.5 | 13.0-15.0 | 3.0-4.0 | 0.75 |
| ER321 | 0.08 | 0.3-0.65 | 1.5-2.5 | 0.03 | 0.01 | 18.5-20.5 | 9.0-10.5 | 0.75 | 0.75 |
| Modelnr. | Treksterkte Rm (Mpa) | Opbringststerkte Rel of Rp0.2 (Mpa) | Ferlinging (%) | Modelnr. | Treksterkte Rm (Mpa) | Opbringststerkte Rel of Rp0.2 (Mpa) | Ferlinging (%) |
| 304 | 550 | -- | 25 | ER309LSi | 510 | 320 | 25 |
| 304L | 510 | -- | 25 | ER316 | 510 | 320 | 25 |
| ER307 | 590 | 350 | 25 | ER316L | 510 | 320 | 25 |
| ER308 | 550 | 350 | 25 | ER316LSi | 510 | 320 | 20 |
| ER308L | 510 | 320 | 25 | ER310 | 550 | 350 | 25 |
| ER308LSi | 510 | 320 | 25 | ER347 | 550 | 350 | 25 |
| ER309 | 550 | 350 | 25 | ER317 | 550 | 350 | 25 |
| ER309L | 510 | 320 | 25 | ER321 | 550 | 350 | 25 |
| TIG- en MIG-lasdraadkomposysje fan roestfrij stiel | ||||||||||
| YB5092-2005 | AWS | Gemyske gearstalling % | ||||||||
| C | Si | Mn | P | S | Cr | Ni | Mo | |||
| H08Cr20Ni9Mn7Si | ER307Si | 0.075 | 0.78 | 6.7 | 0.022 | 0.01 | 19.8 | 8.8 | ||
| H06Cr21Ni10 | ER308 | 0.045 | 0.45 | 1.9 | 0.02 | 0.009 | 20.8 | 9.8 | ||
| H0OCr21Ni10 | ER308L | 0.02 | 0.32 | 1.9 | 0.011 | 0.006 | 20 | 10.2 | ||
| H06Cr21Ni10Si | ER308Si | 0.045 | 0.85 | 1.5 | 0.022 | 0.01 | 20.8 | 9.8 | ||
| H06Cr24Ni13 | ER309 | 0.06 | 0.45 | 1.9 | 0.019 | 0.009 | 24.3 | 13.2 | ||
| H06Cr24Ni13Si | ER309Si | 0.06 | 0.79 | 1.95 | 0.019 | 0.009 | 24.7 | 13.2 | ||
| H03Cr24Ni13 | ER309L | 0.02 | 0.42 | 1.8 | 0.02 | 0.01 | 24.8 | 13.2 | ||
| H03Cr24Ni13Si | ER309LSi | 0.018 | 0.8 | 1.7 | 0.02 | 0.01 | 23.5 | 13.5 | ||
| H21Cr16Ni35 | ER330 | 0.2 | 0.38 | 1.5 | 0.022 | 0.01 | 16.5 | 34.5 | ||
| H06Cr19Ni12Mo2 | ER316 | 0.04 | 0.4 | 1.9 | 0.02 | 0.01 | 19.5 | 11.8 | 2.3 | |
| H06Cr19Ni12Mo2Si | ER316Si | 0.05 | 0.7 | 1.92 | 0.02 | 0.01 | 19.5 | 11.8 | 2.3 | |
| H03Cr19Ni12Mo2 | ER316L | 0.019 | 0.38 | 1.8 | 0.018 | 0.01 | 19.8 | 12.2 | 2.5 | |
| H03Cr19Ni12Mo2Si | ER316LSi | 0.06 | 0.85 | 1.7 | 0.022 | 0.01 | 18.8 | 12.6 | 2.4 | |
| H03Cr17Ni14Mo3 | ER317L | 0.02 | 0.38 | 1.8 | 0.02 | 0.01 | 18.8 | 13.8 | 3.6 | |
| H08Cr19Ni12Mo2Nb | ER318 | 0.06 | 0.42 | 1.5 | 0.022 | 0.01 | 18.5 | 11.8 | 2.3 | |
| H07Cr20Ni34Mo2Cu3Nb | ER320 | 0.06 | 0.4 | 1 | 0.022 | 0.01 | 19.8 | 33.3 | 2.8 | Nb0.7 |
| H02Cr20Ni34Mo2Cu3Nb | ER320L | 0.018 | 0.33 | 1.5 | 0.013 | 0.01 | 19.8 | 33.6 | 2.5 | Nb0.35 |
| H08Cr20Ni10Ti | ER321 | 0.06 | 0.45 | 1.5 | 0.022 | 0.01 | 20.8 | 9.8 | Ti9xC-1.0 | |
| H08Cr21 Ni10Nb | ER347 | 0.055 | 0.48 | 1.8 | 0.021 | 0.008 | 20.8 | 9.8 | Nb1xC-1.0 | |
| H12Cr26Ni21 | ER310 | 0.09 | 0.5 | 1.66 | 0.02 | 0.01 | 25.5 | 20.5 | ||
| H02Cr20Ni25Mo4Cu | ER385 | 0.02 | 0.3 | 1.5 | 0.018 | 0.01 | 20.2 | 24.8 | 4.8 | Cu 1.80 |
| H03Cr22Ni9Mo3N | ER2209 | 0.022 | 0.5 | 0.9 | 0.02 | 0.01 | 22.5 | 8.8 | 3.3 | N0.08-0.20 |
| H04Cr25Ni5Mo3Cu2N | ER2553 | 0.027 | 0.5 | 1 | 0.025 | 0.015 | 24.8 | 5.5 | 3.2 | N0.1-0.25 |
| H1 5Cr29Ni9 | ER312 | 0.09 | 0.38 | 1.5 | 0.022 | 0.01 | 29.5 | 8.5 | ||
| H03Cr24Ni13MoL | ER309L Mo | 0.023 | 0.45 | 1.5 | 0.022 | 0.01 | 23.8 | 13.2 | 2.2 | |
| H05Cr17Ni4Cu4Nb | ER630 | 0.04 | 0.39 | 0.5 | 0.022 | 0.01 | 16.5 | 4.8 | Cu;3 Nb;0.28 | |
| H08Cr26Ni5Mo2 | ER453's | 0.06 | 0.3 | 0.4 | 0.022 | 0.01 | 25.8 | 4.8 | 2.1 | |
| H08Cr21Ni10Mn6 | 0.06 | 0.35 | 5.5 | 0.022 | 0.01 | 20.8 | 9.8 | |||
| H05Cr22Ni11Mn6Mo3VN | ER209 | 0.04 | 0.4 | 4.5 | 0.022 | 0.01 | 21.5 | 10.8 | 2.2 | N;0.20 V;0.18 |
Wenzhou Tianyu Electronic Co., Ltd. waard oprjochte yn 2000. Wy binne al mear as 20 jier dwaande mei de produksje fan laselektroden, lasstangen en lasferbruiksartikelen.
Us wichtichste produkten omfetsje laselektroden fan roestfrij stiel, laselektroden fan koalstofstiel, laselektroden fan leechlegearre stiel, laselektroden fan oerflakken, laselektroden fan nikkel- en kobaltlegearre stiel, lasdraden fan myld stiel en leechlegearre stiel, lasdraden fan roestfrij stiel, gasbeskerme fluxkerndraden, aluminium lasdraden, ûnderdompele bôge-lassdraden, lasdraden fan nikkel- en kobaltlegearre stiel, lasdraden fan messing, TIG- en MIG-lasdraden, wolfraamelektroden, koalstofgutselektroden en oare lasaccessoires en -ferbrûksartikelen.
Wenzhou Tianyu Electronic Co., Ltd. waard oprjochte yn 2000. Wy binne al mear as 20 jier dwaande mei de produksje fan laselektroden, lasstangen en lasferbruiksartikelen.
Us wichtichste produkten omfetsje laselektroden fan roestfrij stiel, laselektroden fan koalstofstiel, laselektroden fan leechlegearre stiel, laselektroden fan oerflakken, laselektroden fan nikkel- en kobaltlegearre stiel, lasdraden fan myld stiel en leechlegearre stiel, lasdraden fan roestfrij stiel, gasbeskerme fluxkerndraden, aluminium lasdraden, ûnderdompele bôge-lassdraden, lasdraden fan nikkel- en kobaltlegearre stiel, lasdraden fan messing, TIG- en MIG-lasdraden, wolfraamelektroden, koalstofgutselektroden en oare lasaccessoires en -ferbrûksartikelen.